Skip to main content

Re: [MW:26581] Re: QW 407.4 Clause requirement

Hi!
Yes weld metal does not come under preview of Qw 407.4 but there is restriction on base metal thk which is 1.1 time T  of test plate of PQR so indirectly autometicaly.applies to weld metal 
Incase of multiprocess PQR.undergoes NR and if the weld thk of each process is more than 19mm in such case each process weld thk qualifies to max thk equal to 1.1T of PQR test plate and  for weld less than 19mm it qualifies 2t of each process
Regards
Hegde Prakash



On Sun, 4 Jun 2017 at 10:42, MW
<raghurambathula@gmail.com> wrote:
even some time interpretation needs interpretation??
in my opinion, QW 407.4 does not apply to weld metal thickness.

On Saturday, 3 June 2017 09:25:35 UTC+4, vijay Katkar wrote:


Dear Sir,

 

Need your help on following issue,

 

I have PQR with 88 mm thickness ( SMAW – 32 mm & SAW -56 mm)and it  has normalizing + stress reliving heat treatment. Generally it is used for dish end long seam (where fiber elongation is more than 5%).

 

As per QW 407.4 Base material thickness T will be qualified 1.1 times of test coupon thickness, in my case it will be 96 mm maximum and deposition thickness will be as per QW 451 table but shall not be more than base metal thickness. As per my assumption SMAW- up to 96mm & SAW- up to 96mm will qualify.

 

As per interpretation IX 83-102. Both thickness will qualify 1.1 times. It means that SMAW will qualify up to 35 mm & SAW -  61 mm. Is this interpretation valid as per latest code requirement?

 

 

I have attached interpretation copy for your reference.


Vijay Katkar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...