Friday, April 1, 2016

Re: [MW:24609] GTAW weld weaving

which edition??

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Fri, Apr 1, 2016 at 11:22 AM, Sathish Jaganathan <sathishjagan80@gmail.com> wrote:
Hi

Please refer ASME SEC II- C page no 133 & 138 (*Notes)

On Thu, Mar 31, 2016 at 4:58 PM, jaya anil <nethalaanil@gmail.com> wrote:
As per Section IX, Weld Weaving is non essential variable for GTAW process. 

As such it is based on your WPS  which was qualified and recorded . If your job is having , Notch Toughness requirement, then dont go for more weaving which will reduce toughness properties. Go with multi layers .

Thanks

On Thu, Mar 31, 2016 at 3:29 PM, simon lawrence <simonlawrence08@gmail.com> wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/757ab274-8b90-4e73-93a9-35e7c078e57f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK2QV3QFiqaSwxrdqcXrstoGNNThQbXqq%3D1YEt-x6G1YyPjRoQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards.....,
J.Sathish
QC Inspector ( Mechanical)
Gulf Petrochemical Services & Trading LLC.
Mob no:-+968-96371006

Alternate Email:- sathishjaganathan@yahoo.com
Oman


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnxsQy5p%2B3g1hN7e%2BKftd8%2BqGgJs10kGL3B_2NuJJHiTWCsWA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePHNKHvwEhjzE8bk%3D9KhtxRwewB%3DPbw-t7utParVJo%3DfQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone