Dear sir
please and the radiography film photo
please and the radiography film photo
From: pkkanishk2006@gmail.com
Sent: 01-04-2016 11:33 AM
To: Materials & Welding
Subject: [MW:24605] 3/4" Tube weld RT
Dear Experts ,
-- I have a situation where external cavity is visible and significant physically on a 3/4" tube weld joint ( welding process - Orbital) , but when we tried to verify through RT DWSI technique its no density variation observed so not able to conclude. Now the vendor is claiming it acceptable , please suggest a way forward and any technique to verify.
Regards
Pratish
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22d82861-95d1-4217-9b2b-6993b901c46b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.