RE: [MW:24279] 2:1 Semi Elipsoidal Dish Head

Hello
Whats is the thickness and material. Please



Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: José Juan Jiménez Alejandro <jjjimeneza@gmail.com>
Fecha:12/02/2016 02:19 PM (GMT-04:30)
Para: materials-welding@googlegroups.com
Cc:
Asunto: [MW:24275] 2:1 Semi Elipsoidal Dish Head

Any of you have a procedure that can provide me to measure 2: 1 Semi ellipsoidal Dish Head, according to the parameters of ASME Section VIII Division 1 (UG-32, UG-79, UG-81).
Thank you!

--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLfzbT26Rh-zA_x6sqPKMky6zXZ0NuWoMzywau9GboorA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...