Tuesday, February 2, 2016

Re: [MW:24210] Procedure qualification for AISI 4130 (Cr-Mo forging)

How can ASME Sec VIII div 1 be construction code for valve repair ?

Please recheck the code.

Prem Nautiyal



Sent from Samsung Mobile


-------- Original message --------
From: Dhamotharan Vaiyapuri
Date:02/02/2016 5:52 PM (GMT+05:30)
To: Materials & Welding
Subject: [MW:24207] Procedure qualification for AISI 4130 (Cr-Mo forging)

Dear Experts,

I want to qualify a procedure for material AISI 4130, in 40 mm thickness, Code of construction is ASME Sec VIII Div 1.

Please advise at what temperature the impact test is to be performed? (no specific client requirement)

The intent to use this WPS for valve repair.

Thanks


V. Dhamotharan

Inspection Engineer,

Doha Qatar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/19211845-f5dc-4b25-960f-a1cf5e36c21d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...