Its normal P1, G2 with MDMT-46. Before PWHT UT carried out on welded elbow. Still vendor agreed to carryout UT after PWHT.

Regards
Yoga

On 2 February 2016 at 12:48, Gurunathan R <saneguru@gmail.com> wrote:
Hi Yoganandhan,

Code doesn't specifically address that NDE has to done before or after PWHT for normal P1 material, some special material it has to be after PWHT

Best Regards,
Gurunathan


On Feb 1, 2016, at 6:34 PM, yoga nandhan <yoganandhan@gmail.com> wrote:

Dear All,

Kindly advice for the requirement of NDE on welded elbows used in the Div.2 vessel, after PWHT of vessel. Is there any clause in Div.2 for NDE exemption for bought out items...

Regards
Yoganandhan.P

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADFD3xRRD%3D8x7sRpZd4%3Dbv0dzQa5ybcMLX2Zi0Lc8e1CRer1fw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/62CD2CA2-6477-46C7-AC39-2BDB35FEB5F9%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards
Yoganandhan.P

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADFD3xTxB2Hztc_m%2B7gn8tQEDQM7j7WHwPaOu_4PXnWApEV%3DVA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone