Re: [MW:24200] Insulating gasket

HI. CHECK ELECTRICAL INSULATION AND TORQUE
 
Atentamente
Agustin Jimenéz
Movil: +52 4881116229
 


El Lunes, 1 de febrero, 2016 6:47:23, Shridev Kurup <shridevk20@gmail.com> escribió:


Dear all
Can anyone help me with precommisionng check list for the piping system where flanges are used dissimilar material and used insulating gasket kit for 2500#  RTJ/RF gaakets.
What are the minimum checks or tests or inspections will be carried out as a part of commissioning to verify or satisfy that installed gaskets functions properly and isolation of dissimilar material is maintained.
Material selection type, instaltion is correct and verified ..exclude those scenarios.

Regards
Shridev
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF7Kwvk_NnFZzC0Eo8YMFL0ZTrtFhCfWTYCUmD3iBuiExhOweg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...