[MW:24266] Sub size Impact test value


Sir,

Can anyone explain to me is this impact value correct or not for MDMT -8.5 Deg C. Materials is P No-1 Group No-2. Applicable code API-650 Edition 2013.

 




Regards
Naz

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b403a36-28c6-4bd5-a8a6-c03c01f3a9e0%40googlegroups.com.