Hi Vishwas,
Would you please provide more details about this grade, UNS No, material specifications etc. The known and popular precipitation hardenable grades are as attached.
Thanks,
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Hamilton, Ontario, Canada
ca.linkedin.com/pub/pradip-goswami/5/985/299
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vishwas Keskar Welding Manager Pune India
Sent: Monday, October 05, 2015 12:13 PM
To: Materials & Welding
Subject: [MW:23663] MDN 11-10 PH STEEL WELDING GUIDLINES
Dear Experts ,
-- Can somebody throw light on welding technology used for welding M D N 11-10 -PH STAINLESS STEEL
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/65e25930-d20d-497e-81a7-7713698d64f0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments