Wednesday, April 1, 2015

Re: [MW:23027] pneumatic test of RF pad of nozzle

Warm Greetings ,

We don't call it Pneumatic Test . We call it Leak test which is done to check weld integrity at the RF pad and nozzle by applying pressure through the vent hole and check the weldment with Snoop solution . 
 

On Tue, Mar 31, 2015 at 11:54 PM, Rahul Chaudhari <navyrahul@gmail.com> wrote:
Dear all ,

Can some one Tell me that why are we take pneumatic test of RF pad of
pressure vessels nozzle???

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V_5nq7hurgbta5XPCe3jx2cs1d3DP6GvUiAmLXD200jVQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuraZ0u8OZvNyFM9Cuf5mrMEA7Qru4WbZsqK2ajkVkMfyQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...