Monday, March 30, 2015

Re: [MW:23017] Dillmax 690 weld cracks

what method was used for joint preparation? gas cutting, grinding , machining ? what is the thk of joint.? can you take a photo of cracked joint and send. my mail id : vanchinaths @gmail.com

On Mon, Mar 30, 2015 at 12:30 PM, RK <krishna.4969@gmail.com> wrote:
Hi..
 
We have used Dillimax 690PE material for our penstocks under construction.
Experienced delayed cracking in welds (after a month or so) in all most all the welds...in all 3 welding processes used SAW, SMAW, FCAW...cracks are only in the welds!!!
Process is PH 100-150 DegC, Interpass 200 Deg C and DHT 200-250 DegC for 3 hrs.
Can anyone have any idea what could be the reasons?? we are in soup...and not able to proceed further..
 
rgds
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/71e1545b-e44d-4786-9afe-6e6d53a90504%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1JH74Nk8OHjeNrxXqWLS%2BMaGmkwvxq3Z-ijdX1QUmyjHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...