Wednesday, March 11, 2015

Re: [MW:22967] Requirements Of PWHT for the Cross Country Pipe Lines - Reg

Hi,
Since your WPS qu
 
Thanks & Regards,alified with PWHT, you can't use this for without PWHT jobs.
Since your construction code doesn't reqire PWHT you have 2 option.
01. Do new WPS/PQR without PWHT
02. If you don't want to prepare new, then follow as per your existing WPS (as your client said)

(Karthik)




On Friday, March 6, 2015 6:40 PM, Anup N K E <nkeanup@gmail.com> wrote:


Refer scope of work,  Isometric drawing and P & ID to find the applicable code.
Section 434.8.9 specifies about PWHT is ANSI B 31.4
Regards,
Anup
On 6 Mar 2015 08:59, "'mv_srinivasan' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Sir,
which design code is used whether ASME 31.4  or ASME 31.8.


Sent from Samsung Mobile


-------- Original message --------
From: Amul Raj
Date:05/03/2015 11:58 (GMT+03:00)
To: materials-welding@googlegroups.com
Subject: [MW:22939] Requirements Of PWHT for the Cross Country Pipe Lines - Reg

Dear Experts,

We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)

Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required 

Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT

What is the remdy for this & hat should we do 

Kindly drop your advise 


Thanks & Warm Regards,

Amul Raj T

QA/QC Welding 

Samsung Engg, KSA  



 




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2f252b05-3866-481c-9fcf-2357a5f0c95e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bx0ck71s8shh6put0pe6ceia.1425578687428%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutYVhgDnOXS2Cx2NuqVxUEtdST1CA3465R6j_3tQOudMUQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...