Dear Experts,

 

Could anyone advise me on the best route to follow regarding plasma cutting of stainless steel, I am aware that this is a welding forum, but it would be interesting to hear from people that use this cutting method and machines in their processes.

 

We are a company that have tube mills. We produce thin walled  stainless steel tubes of various diameters. The material thicknesses we use are 0.3mm, 0.25mm, 0.2mm and 0.15mm.

 

The stainless steel we use are of various grades e.g. 316, 321, etc..

 

We are currently cutting tubes on the fly circumferentially. We have a plasma torch mounted  on a rotating head, and cuts the tube as it passes through the head.

 

The problem we have is something we refer to as 'plasma dust', this is residue of the steel after the cut, this residue sits on the inside of the tube near the cutting edge.

 

We are looking at ways to reduce this 'plasma dust' issue. We are researching new model plasma cutting machines that can cut our tubes with minimum or no 'plasma dust', or some other type of cutting technology.

 

If anyone has experience or information that can help us in this regard, this information will be greatly appreciated.

 

Regards,

 

Naasief

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of umang patel
Sent: 10 March 2015 12:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:22962] Regarding TIG v/s MIG

 

Dear expert

 

I want to do Project On Comparison between MIG welding process v/s TIG welding Process and FCAW welding process v/s GMAW welding process(for steel).

so, i want to research papers , documents regarding this pls send me and guide me.

 

regards,

 

Umang Patel

 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKyp404euYf9RBYJ-O8SwJZ%3DxUVam5VJvBFm_c%2BkrykmKZgdPg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.




This email has been scanned for email related threats and delivered safely by Mimecast.
For more information please visit http://www.mimecast.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...