Re: [MW:22960] difference between ER70 S-6 and ER70 S-3

Hi,

Yes, the impact properties of ER 70S-6 (27 J at -30°C) is better than that of  ER 70S-3 (27 J at -20°C)

Please refer Sec II Part C SFA 5.18

Regards,
LALU
LINKS MIDDLE EAST
ABU DHABI, UAE





On Mon, Mar 9, 2015 at 6:52 PM, 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear expert ;

we have  to weld an ammonia liquid line ( temperature of service -33 °c) with ER 70 S-3 for penetration and E 7018 for filling and cap .

Our client ask to weld with ER 70 S - 6 because of better impact test proprities.

THis is true ?? please give me more details

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/830348253.1966186.1425912751788.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13vd%3DyZ8nFr-%3D8UYbffdG7TZzf%3DVSn9q1aV2YJWf7Okj%3DA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...