Re: [MW:22955] minimum leak path

Dear,

Leak path dimension is not mentioned in ASME section IX.

As per ASME Section IX, QW-193.1.3 Acceptance Criteria — Macro- Examination.

Using a minimum of 10X magnification, the exposed cross sections of the weld shall confirm

(a) minimum leak path dimension required by the design

On polishing & etching the section, the minimum throat thickness or leak path of each weld shall not be less than 0.7t, where t is the nominal wall thickness of the tube.

Regards
 
V.Venkatesan
Velosi- Saudi arabia

On Wed, Mar 4, 2015 at 10:28 AM, venkkatesh krishnan <venkkateshkrishnan@gmail.com> wrote:
Dear Experts,

             Kindly please clarify what is minimum leak path dimension as per QW-193.1.3 and how to calculate, actually my design is groove + fillet weld seal welded as per UW-20

          Groove depth: 2.47mm

          Fillet size: 2.47mm

    thanks in advance.

Regards,
Venkkatesh Gopalakrishnan.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fddf46e9-b5f1-4d57-b085-bb75256cc7b6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABgMRAUL3yZ-KbY9JTxum85Wj8Yohzy2LOYLyRhHa67JvPVu5A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...