Dear Luis Opazo Z
This for your information you pipe API 5L X70 PSL -02
1. For main line welding- Welding processes GMAW - ER80SG (AWS 5.28)
all passes.
2. For Tie-in welding - welding processes STTP(Semi auto ) + FCAW (Semi auto)
Consumable For Root pass - ER70SG (A 5.18) ,Other passes
E81T8G (A 5.29)
3. For Partial Repair – Welding processes FCAW (Semi auto)
Consumable- E81T8G (A 5.29)
4.For through repair - Welding processes SMAW + FCAW(Semi auto)
Consumable For Root –E 6010 (A5.1), For Hot Pass – E8010G (A5.5).
Other passes - E81T8G (A 5.29)
Regards
Madhusoodhanan Nair G (INDIA)
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq70a2-wZGwgtxdVDNkZbk6BRGUnVcWQXXpCRVJiTzBx8A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment