It comes under unassigned material and u have to go with separate PQR qualification for the same. Each unassigned material with its counter part material have to be separately qualified. However some clients accept it to use as group 1 or 2, without any requalifi cation. So take client concurrence.

Sent from my iPhone

On Mar 2, 2015, at 16:31, Siva Chidambaram <mechsivachidambaram@gmail.com> wrote:

Hi friends,
 Kindly clarify my doubt.
 
In AWS D1.1, they have assigned groups for some materials.
I need to know whether we can use the Groups nos of the material if we are using the equivalent material of the assigned one in AWS D1.1 table 3.1.
 
For example. Material EN10025 S275 JR is not assigned in the Group of AWS D1.1 table 3.1. Whether I can assign it as Group 1, since its equivalent material is in Group 1 in AWS D1.1 Table 3.1
 
kindly clarify.
 
Thanks
 
M. Sivachidambaram
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMVetV2ohFdAThXv_W-vKt7dRbx5u6KWE4349EgT_ZjU5A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...