Re: [MW:22934] EN 10204 2.2 Certificate..

Manufacturer's compliance statement certificate against the po requirements and specification requirements is considered enough for EN 10204-2.2. Certificate statement will cover the qty and any other requirements.

If Tc and further test details requested can be considered further assurance of the product quality and manufacturers can demand additional charges against those quality tests if initial po order and terms requirement was only EN10204- 2.2.

Normally all pressure parts are considered 3.1 by majority of the customers.

Regards
Shridev

On 4 Mar 2015 13:44, "Vadivel Mahadevan" <vadivelmahadev@gmail.com> wrote:
>
> Dear Experts,
>
> Can you please throw me an Idea whether we need to match the Quantity for EN10204 2,2 Certificates. 
> Supposedly consider a lot of around 30 nos of a pressure part where customer has requested for EN 10204 2.2 Certification for internals. Whether I am supposed to submit him internals Test certificate to match this 30 nos or a sample TC is sufficient enough.
>
> What is the procedure to raise this issue to EN body?
>
> Thanks and regards
> Vadivel. M

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF7KwvkFVJkH_ek--OPdKfSJ_-jCqF497hMD_wOp_5qBFRZGBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...