Suitable electrode for this combination is E8018-W2

On Mar 4, 2015 2:46 PM, "Vijay" <k.vijayaraj@gmail.com> wrote:
Dear Experts,

We need to qualify a PQR for S355 J2W Corten Steel Plates and I request you to suggest a suitable electrode and provide me a PWPS for S355 J2W.

Thanks in advance.

Sincerely,
Vijay 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMBpsEd-ASMJ2QdVkyeb%2B8hCdJULufvc6O2uwB5X8d_RX33u-A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKYi2-7V8b2RjsZbcL_b6em4EFP2N2v5kK%2B035%3DjOkUgVfT9jw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...