Dear Sir,
 
I have a 2 chemical compositions one is Italian material another one is Brazilan material, Requesting you to conform the grade or any equivalent material in Indian grade.
Italy chemical composition
ELEMENTS           % BY WT
C                                0.243
Si                                0.26
Mn                              1.19
P                                 0.012
S                                 0.008
Cr                                0.32
Ni                                 0.16
Mo                               0.05
HARDNESS HRC:         43.7
Brazil chemical composition
ELEMENTS           % BY WT
C                                0.183
Si                               0.80
Mn                              1.34
P                                0.026
S                                 0.014
Cr                                0.14
Ni                                 0.11
Mo                               0.04
HARDNESS HRC:         41.7
Anyone Please help me....
 
Regards
Vinay

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/044d32c0-698a-47ad-92e3-6bff5608e1c6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...