[MW:23004] Re: ASME Sect IX-QW-405-Position Qualification Ranges

Hi Kunal
 
Addition of position is an essential variable for Hardfacing/ Corrosion resistant overlays. Please refer Table QW-256.1 for GTAW.
 
Thanks and Regards
Harikrishnan
On Wednesday, March 25, 2015 at 11:29:43 AM UTC+8, Kunal Patel wrote:
Dear friend,

Please refer ASME SEC-IX QW-203: Limit of Qualified Position for Procedure. Position is not essential variable for welding procedure except SAW welding process.

Kunal Patel
BVIPL

On Tuesday, 25 March 2014 14:18:59 UTC+5:30, Anban wrote:
Dear Experts

Position only a Supplementary essential variable (ie when CVN-Impact test required).

QW-405.2 A change from any position to the vertical position uphill progression. Vertical‐uphill progression
(e.g., 3G, 5G, or 6G position) qualifies for all positions. In uphill progression, a change from stringer bead to weave
bead. This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature
or when an austenitic material is solution annealed after welding.

QW-405.4 (a) Qualification in the horizontal, vertical, or overhead position shall also qualify for the flat position. Qualification
in the horizontal fixed position, 5G, shall qualify for the flat, vertical, and overhead positions. Qualification in
the horizontal, vertical, and overhead positions shall qualify for all positions. Qualification in the inclined fixed position,
6G, shall qualify for all positions.

I'm looking at some of the WPS/PQRs received from Vendor. 
PQR state that Position Tested/Qualified- 1G
WPS state qualified for all groove and fillet positions?
CVN Tested at -30 deg C.

Based on QW-405.2 & QW-405.4- 1G does not qualify all positions.Only qualified for 1G & 1F.

Plls explain how "This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature
or when an austenitic material is solution annealed after welding." relevant to Positions.


Pls shine some light on this. Thank You.



















































--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b28adefd-9dbd-46ae-a1f1-168fcb9b8e00%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...