[MW:23002] Reg - Etchant for Aluminum material

Dear Experts,

I need certain Aluminum weld samples to be Macro etched .

The grades of Aluminum are ALU 5052 & ALU 1050.

Kindly advice me that which etchant has to be used to reveal proper weld fusion.

Thanks in advance :)

Awaiting experts advice.

With regards,
R.Anand Raj

CSWIP 3.1 Welding Inspector
ASNT LEVEL II 



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACcgZYiij0BgmzV4TQeMOJvogBHDh3dM0nkESHTcCkngywmj2A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...