Dear Experts,

based on the below conversation, 

incase a fabricator owns a PMI machine,

what will be the Tolerance for chemical elements ( base metal and Weld metal )  and what is the accuracy level for calibrating the PMI machine.

Regards,
Saravanan

On Fri, Feb 13, 2015 at 12:37 PM, pradip kumar Sil <pradipsil@gmail.com> wrote:
Follow PFS standard, 10% bilateral tolerance on parent material & 12.5 % tolerance  on weld material. 
Chk composition on ASME SEC II

On Fri, Feb 13, 2015 at 5:12 AM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Experts,

We have done PMION weld joint of INCONEL625 i.e. ENiCrMo-3
Found
Ni -61, Cr-24.6, 25.6, Mo-8.5, Nb -3.37,

Now, As per procedure & code i. e.
Sec II C Cr range is 20-23 given
all other elements are in range.
And PMI analyzer also display Inconel 625.
Please confirm whether it is acceptable or not i.e. chromium %

Best Regards,
Mohit Aggarwal.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOtBHVu5HvuVxdG24WR3uCSsH5sXQkAGkf7C1eLug-r0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DqR-d5rm49p7kE9vPk6i1Qw9iyzBL%2BPq_ufxjCVTEiTw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJ1XUvsWURcPmPaa7jrijoLD9wm2xZFd3%3DMS4s3u2PW%3DA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...