Please if you could send a picture of leakage points.

 

It´s important to categorized the leakage, if it consist in thickness wall loss or maybe cracks/fissure, type.

 

Once you know the kind of defect, you will detect the main cause for leak

 

Regards

 

Miroslav Tadic
Ingeniero  de Integridad
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de Kumar
Enviado el: martes, 10 de febrero de 2015 16:48
Para: materials-welding
Asunto: [MW:22842] SS piping leaking

 

Dear experts,
3" size SS piping (sa 312 tp 304) is found as leaking in few places (near to weld joint, base pipe area etc..).the service is potable water.sub- contractor saying it might be due to high chloride content (830ppm) or  defective material (leaks mostly found in 1 heat no.).which could be more relevant? If for material, what are the tests for confirmations?  Kindly share your views.
Thanks in advance,
Kumar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp-W2fmNQjGMZbaQruOAL7pExs1N4fn8ZNzfQ%3DdHsJOAdg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...