Wednesday, February 11, 2015

Re: [MW:22845] IS IT POSSIBLE TO MAKE SPLIT TEE BY CUTTING ORDINARY TEE

My apologies for a wrong spelling,
I my idea was that if a material is manufactured A234 it will remain A234 even after you cut it, I don't think we need to look for a code citation. Regarding the NDT if its cut by machining no NDT is required again however as per the need the edge of the new half tee can be tested by PT to ensure that its defect free and suitable to weld.

 
With Best Regards,
Umar Rashid Makrani, PMP®

On Mon, Feb 9, 2015 at 12:00 PM, Umar Rashid Makrani <firoz.makrani@gmail.com> wrote:
If you have a tea of ASTM A234 and you cut it into 2 halves. The material is still ASTM A234 so I believe this can be used.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,


On Mon, Feb 9, 2015 at 11:14 AM, afzal ahmed <afzalahmed999@gmail.com> wrote:
Dear Friends please Help me ,
 
We need Split Tee of 6"(SMLS SCH 40 ASTM A234 GR WPB) , but it is not available in market easily ,
1: Is it possible to make Split Tee by cutting ordinary Tee vertically
2: if Yes, then in which STD it is telling
3: & what are the NDT requirements
 
for more clarification See the attached file
 
its very urgent .....
 
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0656b478-8126-4723-92b4-e58408747f3b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyj6SGyCASx8dU0i-Lhp9nqn6MS-C0QdqmMisxLH7D4fFA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...