Monday, February 9, 2015

Re: [MW:22839] IS IT POSSIBLE TO MAKE SPLIT TEE BY CUTTING ORDINARY TEE

But on what basis client will approve it?
which STD?


On Monday, February 9, 2015 at 1:22:24 PM UTC+3, Rana Abdul Rauf wrote:
Either get approval from client or get its approval from design and proceed .

.... No issue
Regards; ar

Umar Rashid Makrani <firoz....@gmail.com> wrote:

If you have a tea of ASTM A234 and you cut it into 2 halves. The material is still ASTM A234 so I believe this can be used.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,


On Mon, Feb 9, 2015 at 11:14 AM, afzal ahmed <afzala...@gmail.com> wrote:
Dear Friends please Help me ,
 
We need Split Tee of 6"(SMLS SCH 40 ASTM A234 GR WPB) , but it is not available in market easily ,
1: Is it possible to make Split Tee by cutting ordinary Tee vertically
2: if Yes, then in which STD it is telling
3: & what are the NDT requirements
 
for more clarification See the attached file
 
its very urgent .....
 
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0656b478-8126-4723-92b4-e58408747f3b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyhA%3DTJ1cFUghZ06pVB5c%2BNb0mVba2FuFcm3k8D3hh9TcA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5a81f1a3-07a9-40c2-a9c2-5ab587c36a1c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...