[MW:22859] Re: SS piping leaking

This is purely MICROBIOLOGICAL INDUCED CORROSION. RESAON IS HIGH CHLORIDE THIS PIN HOLE CREATE WELD HAZ AREA, DUE TO CHROMIUM CARBIDE PRECEPITATION

On Wednesday, February 11, 2015 at 6:22:55 AM UTC+3, sunilkumar kundothara wrote:

Dear experts,
3" size SS piping (sa 312 tp 304) is found as leaking in few places (near to weld joint, base pipe area etc..).the service is potable water.sub- contractor saying it might be due to high chloride content (830ppm) or  defective material (leaks mostly found in 1 heat no.).which could be more relevant? If for material, what are the tests for confirmations?  Kindly share your views.
Thanks in advance,
Kumar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2cde56ef-3afd-460b-a64d-5e8cc8a8d510%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...