RE: [MW:21740] The requirement of Impact Test by process

Dear,
Impact test apply for combine welding process . Together.
Regards,
Ramon Briceno
Metallurgical Engineer


Date: Thu, 28 Aug 2014 05:20:45 -0700
From: aumpiem@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:21737] The requirement of Impact Test by process

Dear Expert 

I had run PQR are combine welding process is API 5L gr.X65 35 mm with PWHT , 

GTAW on root pass about 5 mm , 
FCAW are fill and cap  30 mm,

For impact test should be test as Root pass (GTAW) or not ? Ref. to ASME IX




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...