Wednesday, August 27, 2014

Re: [MW:21723] Bend test was broken on A312 TP 321

Dear 

Material thickness is 18.27 mm and weld deposited is 18.27 mm
location of best test is center of weld

Vào 09:35:59 UTC+7 Thứ tư, ngày 27 tháng tám năm 2014, Mohit Aggarwal đã viết:

What is thk of base metal and process thk you deposited?

Also location of bend test!!

Best Regards,
Mohit Aggarwal.

On 25-Aug-2014 3:04 PM, "nguyen tuan" <tuan...@gmail.com> wrote:

Dear 

Following specification" Where specified in Contractor Standards or by Licensor, fabrication welds in Type 
321/321H or 347/347H stainless steels shall be subject to a thermal stabilization at 
910ºC±10ºC for 4 hours "

Best regards,
Vào 16:12:00 UTC+7 Thứ hai, ngày 25 tháng tám năm 2014, George Dilintas đã viết:

321 is quenched and tempered in order to stabilize the austenite.
Why you did normalizing?

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for Mahendra Arya ---25/08/2014 08:04:12---Dear friend May I know y u have normalizing for 8 hours....Mahendra Arya ---25/08/2014 08:04:12---Dear friend May I know y u have normalizing for 8 hours....

From: Mahendra Arya <mkarya...@gmail.com>
To: material...@googlegroups.com
Date: 25/08/2014 08:04
Subject: Re: [MW:21684] Bend test was broken on A312 TP 321
Sent by: material...@googlegroups.com




Dear friend

May I know y u have normalizing for 8 hours....
Is it any spec or job requirement...

On 23-Aug-2014 11:35 am, "nguyen tuan" <tuanpvecc@gmail.com> wrote:


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...