Re: [MW:21716] Bend test was broken on A312 TP 321

Maybe you don't need to do the normalizing, try to test your procedure in as welded condition, it's possible that some sigma phase is being formed in your PWHT. You must control the ferrite number in the weld as low as possible without hot cracking. If you still consider doing the heating up 900oC, try a rapid cooling instead.

Sergio Muñoz
http://weld-ing.blogspot.com
http://pe.linkedin.com/pub/sergio-antonio-mu%C3%B1oz-pinz%C3%B3n/54/a33/69

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...