Mr. Ansari,

As per table QW-451 if deposited thk is greater than or equal to 19 mm than qualification thk equal to 2 times of base metal thk if BM thk is less than 38 thk,but if BM thk also above 38 than it is 200 mm max. If There is PWHT done than it becomes 1.1 times of BM thk.

Best Regards,
Mohit Aggarwal.

On 18-Jun-2014 2:40 AM, "Ansari intekhab alam" <ansari.ndt@gmail.com> wrote:

Note that
For base metal T ia applicable and for weld deposit t is applicable.
So ur base metal qualified is 2T for all processes but 4 deposit is only 2t.
So
GTAW 10 MM
SMAW 40 MM
FCAW 50 MM
DEAR EXPERTS CORRECT ME IF I M WRONG
CHEERS
Ansari

On 14 Jun 2014 20:29, "rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" <rajesh.mhaske17@gmail.com> wrote:
 
  Dear sir 
       
         PQR WELDING PROCESS : GTAW +SMAW+FCAW
         WELD DEPOSITION THK  a) GTAW :  5 mm
                                                 b) SMAW : 20 mm
                                                 c)  FCAW : 25 mm
       
 As per  QW-451.1 note 3  ,  the SMAW, SAW, GMAW, PAW, and GTAW welding processes only; otherwise per Note (1) or 2 T, or 2t, whichever is applicable.

Can i use above clause for FCAW

    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...