Dear Experts,
We are received ASTM A36M & A537 Cl1 plate materials for tanks fabrication.
At the time of gas cutting plate are automatically bend of the edge portion.
we are taken hardness for checking it's come very less (80-96 BHN).
ASTM A36 is silent about Hardness value.please provide the require Hardness value and it's what base & relation between Hardness & UTS.
Also,please explain why it will do, we are not get any valid reason to reject the plate, as per MTC all value me to ASTM requirement. 

--
Thanks & Regards
Pinaki Boxi.
ISPRL Site
Mob :- +918142322269

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...