[MW:21683] HARDNESS TEST BEFORE AND AFTER PWHT

Hello, please someone clarify me this. 

Regarding hardness tests under ASME B31.3 2010, Table 331.1.1, paragraph 331.1.7. is performing circumferential welds in pipes with 0.844 inch thick ASTM A 106 Gr. B. transport of sour gas. 
The question is what are the criteria for assessing who takes shots hardness before heat treatment and after heat treatment? 
And under that rule or code? 

I appreciate your support by sharing their knowledge 
greetings

Rusbeli r

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...