Re: [MW:21401] QW-.200.4 of ASME Sec. IX- Combination of Procedures

Dear Experts,

So, I think WPS- A is OK or I can make a single WPS combining PQR-A & B. Please confirm.

Thanks & regards,


C. R. GANDHI


From: "rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" <rajesh.mhaske17@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, July 12, 2014 3:26 PM
Subject: Re: [MW:21399] QW-.200.4 of ASME Sec. IX- Combination of Procedures

Dear sir
       WPS :   BASE METAL THK RANGE QUALIFIED :  1.5- 200 mm
                    deposited weld metal qualified  GTAW : 5 mm max  and  SMAW : 200 mm max
                    refer : ASME sec : ix QW-200.4 Combination of Welding Procedures
                             ASME SEC-IX   QW·202.4 Dissimilar Base Metal Thicknesses-
                                                                More than one procedure qualification may be required
                                                                to qualify for some dissimilar thickness combinations.
                                Multiple WPSs With One PQRlMultiple PQRs Refer example      
                                                                 
   .
         
On Thursday, July 10, 2014 5:08:05 AM UTC+5:30, Shridev Kurup wrote:
Please refer Qw 200.2( f ) & 200.4( a)
On 9 Jul 2014 11:05, "Kannayeram Gnanapandithan" <kgpan...@gmail.com> wrote:
no, but two wps can be used in a single joint???

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Tue, Jul 8, 2014 at 6:13 PM, Shridev Kurup <shrid...@gmail.com> wrote:
1.In my opinion PQR A is sufficent enough to weld the thickness groove thickness 12 mm. Detail of the weld   groove was not clear in the drg.  Wps range available 16 mm                                                                      2. For combination Please refer table QW 451.1 notes (1,2) for combination WPS requitements. Please refer QW407.4 specially if higher thk
3. Tension test needs to confirm the requirements of QW-153 only. Regarding the failure appearance it is not a mandatory requirement as sec- ix. Please refer if any project specific requirement.
4. Again if a little more info can be provided I do not feel any harm in it.Pls refer what lab tesile test procedure details about essential requirement for reporting.                                 I hope our group expert will show some more light on it. Waiting for expert comments                                    Regards                                                       shridev
On 6 Jul 2014 14:37, "'CHINTUKUMAR GANDHI' via Materials & Welding" <material...@ googlegroups.com> wrote:
>
> Dear Experts,
>
> Good day to all. 
>
> I have a query for which I need your opinion. Can I make a single WPS combining two PQR as shown below, for weld details attached (dissimilar base metal thk.- 12 mm. to 66 mm., but deposited 't' shall be 12 mm.) or PQR 'A' will be OK? If PQR 'A' is acceptable then provide me the code reference. 
>
> (1) PQR- A
> T- 8 mm., hence Qualified range T 1.6 mm. to 16 mm.
> Process- GTAW for Root Run and SMAW for balance Passes
> t- GTAW- 2.5 mm. & SMAW- 5.5 mm.; Qualified 't' range- GTAW- 5 mm. & SMAW- 11 mm.
>
> (2) PQR- B
> T- 39.5 mm.; hence Qualified T- 5 mm. to 200 mm.
> Process- SMAW
> t- 39.5 mm.; Qualified 't' range 200 mm.
>
> Awaiting for your prompt response.
>
> Thanks & regards,
>
>
> C. R. GANDHI
>
--
To post to this group, send email to material...@ googlegroups.com
To unsubscribe from this group, send email to materials-weld...@ googlegroups.com
For more options, visit this group's bolg at http://materials-welding. blogspot.com/
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
For more options, visit https://groups.google.com/d/ optout.

--
To post to this group, send email to material...@ googlegroups.com
To unsubscribe from this group, send email to materials-weld...@ googlegroups.com
For more options, visit this group's bolg at http://materials-welding. blogspot.com/
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
For more options, visit https://groups.google.com/d/ optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...