As long as the material is P 8 and consumables are SFA 5.9 (+) SFA 5.4 it is OK.
 
 C Sridhar.
 

 

From: Mohit Aggarwal <aggarwalmohit05@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sunday, 29 June 2014 2:44 PM
Subject: Re: [MW:21295] 316L WPS used for 304L.

Yes you can make but all essential variable should remain same...
Regards
Mohit Aggarwal


On 29-Jun-2014 1:23 PM, "S.Mohammed" <mohd52100@gmail.com> wrote:
Dear all
Have WPS for 316L material.with GTAW+SmAW consumable ER316L +E316L-16.
Can i make WPS for 304L.material with GTAW+SMAW consumbale ER304L+E304-15.?
Regards,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...