Sunday, June 29, 2014

Re: [MW:21298] 316L WPS used for 304L.

Yes As it is in the same P No and F No catagory But you have to write the WPS addressing 304L base and E308L welding consumables  with supporting available PQR of 316L
(provided  you do not require to use this WPS for Impact requirement)
Regards
Hegde p.B.


On Sunday, 29 June 2014 2:47 PM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:


Yes you can make but all essential variable should remain same...
Regards
Mohit Aggarwal
On 29-Jun-2014 1:23 PM, "S.Mohammed" <mohd52100@gmail.com> wrote:
Dear all
Have WPS for 316L material.with GTAW+SmAW consumable ER316L +E316L-16.
Can i make WPS for 304L.material with GTAW+SMAW consumbale ER304L+E304-15.?
Regards,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...