This type of requirement is generally raised by the client when they require minimum certification of the material from the manufacturer. Further, this requirement is generally mentioned when providing the Purchase order to the manufacturer and it is clearly state to mention EN10204 TYPE 3.1 on the MTC. 

If your PO to the manufacturer has included this requirement then definitely they should provide with MTC mentioning EN10204 TYPE 3.1 on it along with the manufacturer seal/stamp & signature to you.


Regards,

Kashif Syed,
QA/QC Engineer
Bahrain



On Fri, Jun 27, 2014 at 7:09 PM, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:
Even though it is 'required' by the Client, the 'requirement' shall be in written form and documented!

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar Arasappa

P.S. : Please don't print this e-mail unless you really need to.

--------------------------------------------
On Thu, 26/6/14, Vairamuthu Ramar <vairamuthu78@hotmail.com> wrote:

 Subject: RE: [MW:21265] EN 10204 type 3.1 requirement
 To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
 Date: Thursday, 26 June, 2014, 8:25 PM




 Definitely Yes.
  

  
 Date: Thu, 26 Jun
 2014 11:33:25 +0530
 Subject: [MW:21260] EN 10204 type 3.1 requirement
 From: sadiq.mech@gmail.com
 To: materials-welding@googlegroups.com

 Dear Members,
 Is it mandatory to be written as EN10204 type 3.1
 on MTC if it is required by client?
 Thanks & Regards,
 Mohd. Sadique Sheikh





 --

 To post to this group, send email to
 materials-welding@googlegroups.com

 To unsubscribe from this group, send email to
 materials-welding+unsubscribe@googlegroups.com

 For more options, visit this group's bolg at http://materials-welding.blogspot.com/

 http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

  

 The views expressed/exchnaged in this group are members
 personel views and meant for educational purposes only,
 Users must take their own decisions w.r.t. applicable
 code/standard/contract documents.

 ---

 You received this message because you are subscribed to the
 Google Groups "Materials & Welding" group.

 To unsubscribe from this group and stop receiving emails
 from it, send an email to materials-welding+unsubscribe@googlegroups.com.

 For more options, visit https://groups.google.com/d/optout.





 --

 To post to this group, send email to
 materials-welding@googlegroups.com

 To unsubscribe from this group, send email to
 materials-welding+unsubscribe@googlegroups.com

 For more options, visit this group's bolg at http://materials-welding.blogspot.com/

 http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

  

 The views expressed/exchnaged in this group are members
 personel views and meant for educational purposes only,
 Users must take their own decisions w.r.t. applicable
 code/standard/contract documents.

 ---

 You received this message because you are subscribed to the
 Google Groups "Materials & Welding" group.

 To unsubscribe from this group and stop receiving emails
 from it, send an email to materials-welding+unsubscribe@googlegroups.com.

 For more options, visit https://groups.google.com/d/optout.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards,


Syed Kashif Farhan
QA/QC Engineer,
Ramsis Engineering,
Bahrain

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...