Pls. find below the answer which is in red color.
Date: Fri, 27 Jun 2014 10:12:32 +0530
Subject: [MW:21274] gain size of stainless steel of material A 350 LF2 of austenitic grade
From: pbrijesh103@gmail.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Date: Fri, 27 Jun 2014 10:12:32 +0530
Subject: [MW:21274] gain size of stainless steel of material A 350 LF2 of austenitic grade
From: pbrijesh103@gmail.com
To: materials-welding@googlegroups.com
Dear Sir,
my question regarding to gain size of austenitic stainless steel material of A350 LF2
1) how to check gain size of above material?????? - As per method ASTM E112 - Testing facility available in all metallurgical testing labs.
2) what is acceptance criteria for gain size??? - The project specification says the accetable grain size. Usually finer grain size products are preferred by most of the services.
3) which gain size check Austenitic or ferrite ????? - There is no difference in checking Austenitic or ferritic steels. It is the test to determine the size of the grain the product has irrespective of ferrite, austenite, martensite or whatever may be the structure.
--
Thanks & Regard's
Brijesh Patel
Brijesh Patel
Engineer
cell no.:- +91 9727013016
IRCLASS Systems & Solutions Pvt. Ltd.
(Subsidiary of Indian Register of Shipping)
301,302,303, Sakar Complex, 3rd Floor, Old Padra road,
Malhar Point, Haribhakti Extension, Baroda-390007
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments