Re: [MW:21246] I. D. MACHINING/ BORING OF SA 106 GR. B PIPES

moreover please refer UW-9 (c).

Thanks,
Vishal Sharma


On Tue, Jun 24, 2014 at 10:58 AM, Vishal Sharma <vishalsharma.sharma225@gmail.com> wrote:
Mr. Gandhi,

Taper transition is not preferable in this case as thickness diff is less. You have to machined up to required schedule.

Thanks & Regards,
Vishal Sharma
(Mo.)  +91-8905999951 


On Mon, Jun 23, 2014 at 11:11 PM, Satish <shahsatish34@gmail.com> wrote:
Dear Gandhi

You have to do 1:3 taper in pipe for matching with wnrf flange id

Satish Shah
QCM
Sent via Micromax


'CHINTUKUMAR GANDHI' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear Experts,

Good day to all. I need your experts' advise for an issue. In ASME U Stamp jobs, may we bore/ machine the I.D. of SA 106 Gr. B Pipes from higher schedule to lower schedule, to match with W.N. Flnage I.D? Actually, we required 8" NPS Sch. 30 pipe and available with us 8" NPS Sch. 40. 

If no, please give me the code reference.

Awaiting for your prompt response.

Thanks & regards,

C. R. GANDHI
(QCM)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...