Monday, June 23, 2014

Re: [MW:21239] RT mandatory for PQR

Again, you will have to refer client's applicable spec. If specified in those docs., then it is required.

Thanks & regards,

C. R. GANDHI


From: "george.dilintas@gr.bureauveritas.com" <george.dilintas@gr.bureauveritas.com>
To: materials-welding@googlegroups.com
Sent: Monday, June 23, 2014 5:41 PM
Subject: Re: [MW:21236] RT mandatory for PQR

Not, if ASME section IX is applicable.
Yes in case EN standard is applicable
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor


I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
(See attached file: Dilintas_George.vcf) This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...