Re: [MW:21233] 316L new pipe to old pipe for Pump

Dear mus.hawa,

Your question is you want to weld the old SS316L pipe to new SS316L pipe, am i correct?

I have not experienced any such issue in these type of welding in refinery or petrochemical industry. Also SS316L is a non magnetic material then issues of magnetic flow will not take place.


Regards,


On Mon, Jun 23, 2014 at 6:44 AM, 'mus.hawa' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Expert,

Below is my situation under brown field offshore HUC work :

1. The existing pipe is 316L sch.S10s
2. The new pipe also 316L sch.10s

My query :

What will happen during the welding in term of the fussion issue. Somebody said, the fussion will be affected due so call magnet flow in the existing pipe.


Please advise if this statement is correct. Also, please advise what is the way forwars to proceed with this welding job.


Rgds,


Sent from Samsung Mobile

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
----------------------
Hareesh K V
+91-9447625012


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...