Hi,

Concern is over the minimum tensile properties for the welding consumable, the minimum for the welding consumable is 480-490 Mpa, where as for base material it is 550 minimum,, the difference of 60-70 Mpa is noted between these two minimum specified tensile values, the vendor proposal is to test the consumable to meet the base metal property, whether it is acceptable.(E7018-1/ER70S2/EH12K)



Thanks'
With Regards'
Ganesh
--------------------------------------------
On Fri, 20/6/14, 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Subject: Re: [MW:21197] Selection of consumable for SA537 CL2 bullets
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Friday, 20 June, 2014, 2:54 PM

Hi!Yes the
consumable you have selected will give you the required
results (Impact value will be as per code using low heat
input  and hardness value can be achieved with proper
preheating of weld joint say min 125
C)RegardsHegde p.B.

On Friday, 20 June 2014 12:49 PM, 'GANESH
GANESH' via Materials & Welding
<materials-welding@googlegroups.com> wrote:


Hi,

suggestion required for slection fo welding comsumables for
AS 537 CL 2 material.

Requirments:

Design ; ASME SEC VIII DIV 2

Material: SA 537 CL2

MDMT : -35 C

PWHT : NO

Thk Shell : 32 mm

Carbon equivalent Max : 0.43

Hardness ; Less Than 248 HV 10

Process / GTAW/SMAW/SAW/FCAW

Whether E7018-1/ER70S2/EH12K can be tested at required
condtions for base metal and can be used or not.



Regards'
Ganesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members
personel views and meant for educational purposes only,
Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
---
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.







--

To post to this group, send email to
materials-welding@googlegroups.com

To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

 

The views expressed/exchnaged in this group are members
personel views and meant for educational purposes only,
Users must take their own decisions w.r.t. applicable
code/standard/contract documents.

---

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...