Friday, June 27, 2014

[MW:21274] gain size of stainless steel of material A 350 LF2 of austenitic grade

Dear Sir,

my question regarding to gain size of austenitic stainless steel material of  A350 LF2

1) how to check gain size of above material?????? 
2) what is acceptance criteria for gain size???
3) which gain size check Austenitic or ferrite ?????

--
Thanks & Regard's

Brijesh Patel
Engineer
cell no.:- +91 9727013016
IRCLASS Systems & Solutions Pvt. Ltd.
(Subsidiary of Indian Register of Shipping)
301,302,303, Sakar Complex, 3rd Floor, Old Padra road,
Malhar Point, Haribhakti Extension, Baroda-390007

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...