Friday, June 20, 2014

[MW:21202] AWS D1.1 -2010-Table 4.5 # 31-Clarification


Dear Sirs

31) A change in groove type (e.g., single-V to double-V), except qualification of any CJP groove weld qualifies for any groove detail
conforming with the requirements of 3.12 or 3.13

Query
PQR qualified with Single-V in 3G Position ( CVN Tested at -40deg C, Weld Process-FCAW,Test Coupon Thk- 25,4mm ).
Can i use this PQR to weld any joint weld groove detail conforming with the requirements of 3.12 or 3.13?

Anyone have AWS Interpretation on this subject?

Thanks in advance to all members.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...