Dear
Referance to below mail please refer UCS-56 ( Refer Given Note No : 2 (c ) 3
Vijay Malusare
Vijay Malusare
---------- Forwarded message ----------
From: Malusare Vijay <vijaymalusare07@gmail.com>
Date: Wed, Jun 25, 2014 at 8:57 AM
Subject: Re: [MW:21249] Post weld heat treatment for blind flange of manhole when lethal service.
To: materials-welding@googlegroups.com
Dear
From: Malusare Vijay <vijaymalusare07@gmail.com>
Date: Wed, Jun 25, 2014 at 8:57 AM
Subject: Re: [MW:21249] Post weld heat treatment for blind flange of manhole when lethal service.
To: materials-welding@googlegroups.com
Dear
As per my knowledge it is required . i come back with proper code referance.
vijay Malusare
On Tue, Jun 24, 2014 at 5:05 PM, ji Ch <jinsuok21@gmail.com> wrote:
Sir.--I've question for this subject.In the ASME Sec.VIII Div.1,The vessel fabricated by carbons steel, and it applied lethal service, so it need post weld heat treatment refer to UW-2 (a)In this case, for blind flange of manhole, davit hinge welded to side portion of blind flange with over 16mm weld thickness of fillet weld.is this blind flange also required post weld heat treatment ? or not ?
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments