--Dear experts,
Please guide me regarding following query:
We are leading fabricator of Al light weight vessels utilizing GMAW-P process. However, we found extensive porosity problems in most of times during 2G and 4G positional welding only when utilizing 99.995% Ar as a shielding gas. In 3G and 1G position seam is getting clear with no indication. We are also using He+Ar as a shielding gas & level of porosity drastically decrease due very known technical reason " getting hot arc welding".
However due to some constraints for short span of time, we are not able to utilize He+Ar for all seams & have to use Ar as shielding gas.
In view if above please suggest how to effectively utilize Ar shielding gas without RT failure, particular to welding in 2G and 4G positions.
Base Metal: AA5083
Filler Wire: ER5183
Thickness: 4 mm
Process: GMAW-P
Shielding Gas: 99.995% Ar with moisture content <2 ppm.
WPS parameters
I-90-120 AMP (2G position)
V-18-19 V
Travel Speed-350-450 mm/min
Regards,
Maulik H. Thakkar
Welding Engg & Metallurgist
L&T, Hazira, Surat
09924732922
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments