Arunabh,
                 Since your service is liquified gas, it wise enough to do pneumatic test rather than hydrotest. Criteria would be ASME Section Viii.


2014-05-28 17:40 GMT+04:00 ARUNABH BERA <bonjoe23@gmail.com>:
Dear Sir
Generally for IBR Line we do Hydrotesting, however, in one of our utility package (Cryogenic Nitrogen Separation Plant), the enitre loop is pneumatically tested and we have one steam line (LP Steam) for Steam bath vaporizer. The contractor is insisting to go for Pneumatic testing because of non availability of pumps, can i allow him to carry Pneumatic testing.
If Yes, then as per which code and if no, the it is requested to kindly throw some light regarding rejection criteria
Warm regards
Arunabh 
Engineers India Limited

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...