Re: [MW:20905] Re: Diff. between WPS of SEC-IX and AWS D1.1

AWS D1.1 is more stringent than ASME sec 9 regarding position and so on . Ref 4.1.1.2

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Wed, May 28, 2014 at 8:50 AM, Shaik Basha <shaik8008@gmail.com> wrote:
Dear Ramesh,

WPSs qualified to ASME IX code is allowed for AWS D1.1 welding with consent of buyer as stated in AWS D1.1 - 2010 clause 4.2.1.2.

Moreover, the structure designed as per AWS will not be subjected to similar type of integrity tests as per ASME Sec VIII/B31.3/31.1 because ASME is for pressure vessels, boilers etc.

Hope this will help.

On Friday, 6 May 2011 13:54:15 UTC+4, Ramesh wrote:

Dear Experts,

 

Greetings,

 

I have one basic question about WPS.

 

Please share your valuable opinions with me that Difference between qualification of WPS with AWS D1.1 and ASME -IX.

 

Can we use the WPS qualified with SEC-IX for steel structure and vise versa?

 

 

Thanks,
With Best Regards,
Ramesh Barot
Cell+919978917399

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...