Monday, May 26, 2014

Re: [MW:20883] LTCS wps revised to CS

Dear Mohammed,
 
"A" Number is an Essential Variable.
 
 Please check  the weld metal chemical composition.
 
Additional elements added in the table QW-440 in 2013 Edition
 
Regards,
S.Veloumany
 

From: S.Mohammed <mohd52100@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, May 26, 2014 8:21 AM
Subject: [MW:20879] LTCS wps revised to CS

Dear all
Have WPS P1G1 to P1G1
for LTCS 333 gr6  with ER80Ni2.
Thk 1.5 to 11
Can i change/revised to WPS P1G1 to P1G1
For A106 grB with ER 70S2.
without PQR qualification.
Since both P n F number not.changed.
Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...