Hi!
What is the T/Tsht joint constrction Whether it is expanded or Strength weld joint ?
ii)Why do you want to heat treat Whole Eqpt ? Does CS Gr 70 shell thk is more than 38mm thk if not
ii) You can get approval for T/tsht weld joint for Local SR by electrical heating
iii) As per ASME code Sec VIII Div 1 You can reduce the PWHT soaking temp with increasing soaking time  Refer code UCS 56
Regards
Hegde P.B.
 
On Monday, 19 May 2014 4:15 AM, Rajesh <mrinmeghnsk@gmail.com> wrote:


Dear All,

We are constructing an heat exchanger which has fixed tubesheet welded to shell.

Shell Material SA 516 Gr 70
Tube Material - Cu Ni 90:10
Tubesheet - SA 266 claded with CU Ni 90:10

Customer is demanding PWHT for complete heat exchanger due to process. But we have fear for failure of tube bundle after PWHT due to differential thermal expansion.

Please comment if CODE has any reference to this?

Rajesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...